1. Review data on AES 1-4 fabrication, processing, and testing.
2. Discuss possible causes for limited cavity performance.
3. Review and recommend any changes for future fabrication procedures and schedule.
4. Recommend future processing and measurement plans for AES 1-4.
Weld prep and machining, weld machine & procedures, time history, inspection & QA/QC at AES. Any data specific to bad cells. Present AES fabrication procedure and schedule.
Speaker:
Rathke
10:45
break
Session II
4
Material, RRR and RRR at weld data, eddy current scanning. Any data specific to bad cells.
Speaker:
Cooley
Slides
5
Discussion of procedures, measurements, possible multipacting, etc
Speaker:
Kneisel
6
Titanium oven treatment. Past results at Cornell, DESY, and JLab.
What should we expect & where could we do it on these cavities?
Speaker:
Hasan/ Lutz
Slides
7
Mechanical polish of welds
Helen described some e-mail correspondence with Kenji Saito
Speaker:
Edwards
Slides
8
Summary of temperature mapping developments
Speaker:
Ciovati
Slides
9
Plan future preparation and testing of AES cavities